螺旋钢管由于其强度高且能承受外部压力,这种管道被广泛用于地下水管道。管道由热轧钢卷带制成,呈螺旋状。用于制造这些管道的螺旋焊接工艺赋予了它们优异的结构完整性,使其成为地下应用的理想选择。
| 标称外径 | 标称壁厚(毫米) | ||||||||||||||
| 毫米英寸 | 6.0 | 7.0 | 8.0 | 9.0 | 10.0 | 11.0 | 12.0 | 13.0 | 14.0 | 15.0 | 16.0 | 18.0 | 20.0 | 22.0 | |
| 单位长度重量(kg/m) | |||||||||||||||
| 219.1 | 8-5/8 | 31.53 | 36.61 | 41.65 | |||||||||||
| 273.1 | 10-3/4 | 39.52 | 45.94 | 52.30 | |||||||||||
| 323.9 | 12-3/4 | 47.04 | 54.71 | 62.32 | 69.89 | 77.41 | |||||||||
| (325) | 47.20 | 54.90 | 62.54 | 70.14 | 77.68 | ||||||||||
| 355.6 | 14 | 51.73 | 60.18 | 68.58 | 76.93 | 85.23 | |||||||||
| (377.0) | 54.89 | 63.87 | 72.80 | 81.67 | 90.50 | ||||||||||
| 406.4 | 16 | 59.25 | 68.95 | 78.60 | 88.20 | 97.76 | 107.26 | 116.72 | |||||||
| (426.0) | 62.14 | 72.33 | 82.46 | 92.55 | 102.59 | 112.58 | 122.51 | ||||||||
| 457 | 18 | 66.73 | 77.68 | 88.58 | 99.44 | 110.24 | 120.99 | 131.69 | |||||||
| (478.0) | 69.84 | 81.30 | 92.72 | 104.09 | 115.41 | 126.69 | 137.90 | ||||||||
| 508.0 | 20 | 74.28 | 86.49 | 98.65 | 110.75 | 122.81 | 134.82 | 146.79 | 158.69 | 170.56 | |||||
| (529.0) | 77.38 | 90.11 | 102.78 | 115.40 | 127.99 | 140.52 | 152.99 | 165.43 | 177.80 | ||||||
| 559.0 | 22 | 81.82 | 95.29 | 108.70 | 122.07 | 135.38 | 148.65 | 161.88 | 175.04 | 188.17 | |||||
| 610.0 | 24 | 89.37 | 104.10 | 118.77 | 133.39 | 147.97 | 162.48 | 176.97 | 191.40 | 205.78 | |||||
| (630.0) | 92.33 | 107.54 | 122.71 | 137.83 | 152.90 | 167.92 | 182.89 | 197.81 | 212.68 | ||||||
| 660.0 | 26 | 96.77 | 112.73 | 128.63 | 144.48 | 160.30 | 176.05 | 191.77 | 207.43 | 223.04 | |||||
| 711.0 | 28 | 104.32 | 121.53 | 138.70 | 155.81 | 172.88 | 189.89 | 206.86 | 223.78 | 240.65 | 257.47 | 274.24 | |||
| (720.0) | 105.65 | 123.09 | 140.47 | 157.81 | 175.10 | 192.34 | 209.52 | 226.66 | 243.75 | 260.80 | 277.79 | ||||
| 762.0 | 30 | 111.86 | 130.34 | 148.76 | 167.13 | 185.45 | 203.73 | 211.95 | 240.13 | 258.26 | 276.33 | 294.36 | |||
| 813.0 | 32 | 119.41 | 139.14 | 158.82 | 178.45 | 198.03 | 217.56 | 237.05 | 256.48 | 275.86 | 295.20 | 314.48 | |||
| (820.0) | 120.45 | 140.35 | 160.20 | 180.00 | 199.76 | 219.46 | 239.12 | 258.72 | 278.28 | 297.79 | 317.25 | ||||
| 864.0 | 34 | 147.94 | 168.88 | 189.77 | 210.61 | 231.40 | 252.14 | 272.83 | 293.47 | 314.06 | 334.61 | ||||
| 914.0 | 36 | 178.75 | 200.87 | 222.94 | 244.96 | 266.94 | 288.86 | 310.73 | 332.56 | 354.34 | |||||
| (920.0) | 179.93 | 202.20 | 224.42 | 246.59 | 286.70 | 290.78 | 312.79 | 334.78 | 356.68 | ||||||
| 965.0 | 38 | 188.81 | 212.19 | 235.52 | 258.80 | 282.03 | 305.21 | 328.34 | 351.43 | 374.46 | |||||
| 1016.0 | 40 | 198.87 | 223.51 | 248.09 | 272.63 | 297.12 | 321.56 | 345.95 | 370.29 | 394.58 | 443.02 | ||||
| (1020.0) | 199.66 | 224.39 | 249.08 | 273.72 | 298.31 | 322.84 | 347.33 | 371.77 | 396.16 | 444.77 | |||||
| 1067.0 | 42 | 208.93 | 234.83 | 260.67 | 286.47 | 312.21 | 337.91 | 363.56 | 389.16 | 414.71 | 465.66 | ||||
| 118.0 | 44 | 218.99 | 246.15 | 273.25 | 300.30 | 327.31 | 354.26 | 381.17 | 408.02 | 343.83 | 488.30 | ||||
| 1168.0 | 46 | 228.86 | 257.24 | 285.58 | 313.87 | 342.10 | 370.29 | 398.43 | 426.52 | 454.56 | 510.49 | ||||
| 1219.0 | 48 | 238.92 | 268.56 | 298.16 | 327.70 | 357.20 | 386.64 | 416.04 | 445.39 | 474.68 | 553.13 | ||||
| (1220.0) | 239.12 | 268.78 | 198.40 | 327.97 | 357.49 | 386.96 | 146.38 | 445.76 | 475.08 | 533.58 | |||||
| 1321.0 | 52 | 291.20 | 323.31 | 327.97 | 387.38 | 449.34 | 451.26 | 483.12 | 514.93 | 578.41 | |||||
| (1420.0) | 347.72 | 355.37 | 416.66 | 451.08 | 485.41 | 519.74 | 553.96 | 622.32 | 690.52 | ||||||
| 1422.0 | 56 | 348.22 | 382.23 | 417.27 | 451.72 | 486.13 | 520.48 | 554.97 | 623.25 | 691.51 | 759.58 | ||||
| 1524.0 | 60 | 373.38 | 410.44 | 447.46 | 484.43 | 521.34 | 558.21 | 595.03 | 688.52 | 741.82 | 814.91 | ||||
| (1620.0) | 397.03 | 436.48 | 457.84 | 515.20 | 554.46 | 593.73 | 623.87 | 711.11 | 789.12 | 867.00 | |||||
| 1626.0 | 64 | 398.53 | 438.11 | 477.64 | 517.13 | 556.56 | 595.95 | 635.28 | 713.80 | 792.13 | 870.26 | ||||
| 1727.0 | 68 | 423.44 | 465.51 | 507.53 | 549.51 | 591.43 | 633.31 | 675.13 | 758.64 | 841.94 | 925.05 | ||||
| (1820.0) | 446.37 | 492.74 | 535.06 | 579.32 | 623.50 | 667.71 | 711.79 | 799.92 | 887.81 | 975.51 | |||||
| 1829.0 | 72 | 493.18 | 626.65 | 671.04 | 714.20 | 803.92 | 890.77 | 980.39 | |||||||
| 1930.0 | 76 | 661.52 | 708.40 | 755.23 | 848.75 | 942.07 | 1035.19 | ||||||||
| (2020.0) | 692.60 | 741.69 | 790.75 | 888.70 | 986.41 | 1084.02 | |||||||||
| 2032.0 | 80 | 696.74 | 746.13 | 795.48 | 894.03 | 992.38 | 1090.53 | ||||||||
| (2220.0) | 761.65 | 815.68 | 869.66 | 977.50 | 1085.80 | 1192.53 | |||||||||
| (2420.0) | 948.58 | 1066.26 | 1183.75 | 1301.04 | |||||||||||
| (2540.0) | 100 | 995.93 | 1119.53 | 1242.94 | 1366.15 | ||||||||||
| (2845.0) | 112 | 1116.28 | 1254.93 | 1393.37 | 1531.63 | ||||||||||
笔记:
1. 也可提供公称外径和公称壁厚介于表中相邻尺寸之间的钢管,但须签订合同。
2. 表格中括号内的标称外径为保留直径。
使用螺旋钢最重要的方面之一是地下水管焊接工艺必须符合规范。焊接是通过施加热量和压力将两个金属部件连接起来的过程。对于地下输水管道而言,焊接质量直接影响管道的整体完整性和可靠性。
恰当的管道焊接工艺螺旋钢管的焊接涉及几个关键步骤。首先,待焊接管道的表面必须清洁,无任何污染物,例如灰尘、油污或油漆。这可以确保焊缝牢固,且不含任何可能影响其强度的杂质。
接下来,必须严格控制焊接参数,例如热输入、焊接速度和焊接技术,以获得高质量的焊缝。使用合适的焊接材料和焊接技术对于防止气孔、裂纹或未熔合等缺陷至关重要,这些缺陷会影响焊缝的完整性。
此外,对于用于地下水管道的螺旋钢管,正确的预热和焊后热处理工艺至关重要。预热有助于降低开裂风险并提高整体焊接质量,而焊后热处理则可消除残余应力并确保整个焊接区域微观结构的均匀性。
此外,采用自动化焊接工艺和无损检测等先进焊接技术,可以进一步提高焊接质量和可靠性。这些技术有助于确保焊接接头达到必要的强度和质量标准,从而保障地下水管线的长期性能。
总之,正确的管道焊接工艺对于确保地下水管线所用螺旋钢管的完整性和使用寿命至关重要。遵循必要的焊接参数、技术和质量控制措施,可以显著降低焊接缺陷和故障的风险。最终建成可靠耐用的地下水管线,经得起时间的考验,并提供安全高效的供水服务。对于地下水管线而言,投资于完善的焊接方案是确保管道整体可靠性和使用寿命的关键步骤。